Our site saves small pieces of text information (cookies) on your device in order to deliver better content and for statistical purposes. You can disable the usage of cookies by changing the settings of your browser. By browsing our site without changing the browser settings you grant us permission to store that information on your device.
I agree, do not show this message again.A study of growth kinetics and distribution of χ precipitates in an induction-aged nickel-base superalloy
S. SOLEIMANI1, A. ABDOLLAH-ZADEH1,* , A. SAMADI1, H. ASSADI1
Affiliation
- Department of Materials Engineering, Tarbiat Modares University, P.O. Box: 14115-143, Tehran, Iran
Abstract
This paper focuses on age hardening behavior of a Ni-based superalloy, during induction and conventional resistance aging. Particular emphasis is placed on the characterization of γ' precipitates, using light laser scattering (LLS), scanning electron microscopy (SEM) and image analysis. The results indicate that the growth of χ' precipitates in the induction-aged samples is considerably faster than that in the conventionally treated ones. This could imply the existence of an additional effect by induction on the growth kinetics of χ' precipitates in this alloy..
Keywords
Ni-based superalloy, Induction aging, Precipitation, Size distribution.
Submitted at: Nov. 14, 2006
Accepted at: June 15, 2007