Our site saves small pieces of text information (cookies) on your device in order to deliver better content and for statistical purposes. You can disable the usage of cookies by changing the settings of your browser. By browsing our site without changing the browser settings you grant us permission to store that information on your device.
I agree, do not show this message again.Hard superalloy layers
I. VIDA-SIMITI1,* , N. JUMATE1, R.D. KNOBLOCH1
Affiliation
- Technical University of Cluj - Napoca, Romania, 400641 Cluj Napoca, Bd. Muncii nr.103-105
Abstract
The vacuum coated green iron powder compacts with high-hardness layers of NiCrSiBC powders were prepared. Diffusioncoated layers have been obtained by compacting at atmospheric pressure. The microstructure, the hardness and microhardness of the coated layers in the diffusion zone and a diffusion model for carbon steel coated with NiCrSiBC superalloys are presented. The samples coated in a vacuum at the temperature of 1100°C (liquid phase sintering) have the lowest interface porosity and hardness between 700 – 1100 HV. The interdiffusion of nickel in iron substrate and iron in superalloy caused a good adhesion of the layer..
Keywords
Coated layers, Superalloy powder, Compacting at atmospheric pressure.
Submitted at: Oct. 12, 2008
Accepted at: Dec. 10, 2008