Our site saves small pieces of text information (cookies) on your device in order to deliver better content and for statistical purposes. You can disable the usage of cookies by changing the settings of your browser. By browsing our site without changing the browser settings you grant us permission to store that information on your device.
I agree, do not show this message again.Surface analysis of some amphiphile polyurethanes
D. FILIP1,* , S. VLAD1, D. MACOCINSCHI1
Affiliation
- Department of Physical Chemistry of Polymers, “Petru Poni” Institute of Macromolecular Chemistry, Aleea Gr. Ghica Voda 41 A, 700487, Iasi, Romania
Abstract
Amphiphile polymers find widespread applications because of their unique ability to self-assemble and modify interfacial properties. Smart polymers have very promising applications in the biomedical field as delivery systems of therapeutic agents, tissue engineering scaffolds, cell culture supports, bioseparation devices, and sensor or actuators systems. Polyurethanes and polyurethane-ureas based on Pluronic macrodiols have been prepared. The morphological and selfassembly characteristics were tuned in function of the structural parameters related to the soft matrix and H-bonding. HF plasma was employed to change the interfacial characteristics. The plasma action was evaluated by contact angle measurements. SEM and AFM analyses evidenced the microheterogeneous morphology and the self-assembling behaviour..
Keywords
Polyurethanes, Amphiphile polymer, Contact angle, Surface tension.
Submitted at: March 13, 2009
Accepted at: May 28, 2009
Citation
D. FILIP, S. VLAD, D. MACOCINSCHI, Surface analysis of some amphiphile polyurethanes, Journal of Optoelectronics and Advanced Materials Vol. 11, Iss. 5, pp. 681-688 (2009)
- Download Fulltext
- Downloads: 337 (from 283 distinct Internet Addresses ).