Our site saves small pieces of text information (cookies) on your device in order to deliver better content and for statistical purposes. You can disable the usage of cookies by changing the settings of your browser. By browsing our site without changing the browser settings you grant us permission to store that information on your device.
I agree, do not show this message again.The effect of the additives and sintering temperature on the structure and humidity sensitivity of a spinel ferrite
N. REZLESCU1,* , F. TUDORACHE1, E. REZLESCU1, P. D. POPA1
Affiliation
- National Institute of Research and Development for Technical Physics, B-dul D. Mangeron 47, Iasi
Abstract
The humidity-sensitive characteristics of MgZn ferrite as a function of the additive type and sintering temperature are investigated. As dopants are used CaCl2, KCl, LiCl and NaCl. The microstructure is dependent upon the sintering temperature and additive kind. All samples exhibit a significant decrease in the specific resistance in the humidity interval 33% RH – 98%RH. The KCl doped ferrite, characterized by higher porosity, shows a shorter response time (3 – 4 minutes) than that of the CaCl2 doped sample (of about 6 minutes)..
Keywords
Spinel ferrite, Chlorides, Microstructure, Humidity sensitivity, Response time.
Submitted at: Feb. 16, 2008
Accepted at: Aug. 28, 2008
Citation
N. REZLESCU, F. TUDORACHE, E. REZLESCU, P. D. POPA, The effect of the additives and sintering temperature on the structure and humidity sensitivity of a spinel ferrite, Journal of Optoelectronics and Advanced Materials Vol. 10, Iss. 9, pp. 2386-2389 (2008)
- Download Fulltext
- Downloads: 23 (from 22 distinct Internet Addresses ).